Felt for Ironing & Embossing Process
Felt for Ironing & Embossing Process | ||
Machine Speed (m/min) | 6 ~ 20 | 5 ~ 10 |
Thickness (mm) | 10 ~ 13 | 13 ~ 14 |
Density (g/m3) | 0.52 | 0.55 |
Composition | 50% wool + 50% synthetic fiber | 40% wool + 60% synthetic fiber |
Weight (g/m2) | 5200 ~ 6750 | 7100 ~ 7650 |
Temperature (℃) | < 140 | < 140 |
Characteristics:
Speical surface finishing
Good guild and stable dimenssion
Anti-static
Without marking joint